Mostrar el registro sencillo del ítem
Obtaining building plaster used in building for forming ceiling, involves mixing recycled slag, additives and water in a blast furnace to obtain a homogeneous material
| dc.contributor.author | Rodríguez Sáiz, Ángel | |
| dc.contributor.author | Manso Villalain, J. M. | |
| dc.contributor.author | Gadea Sáinz, Jesús | |
| dc.contributor.author | Gutiérrez González, Sara | |
| dc.contributor.author | Junco Petrement, Carlos | |
| dc.contributor.author | Calderón Carpintero, Verónica | |
| dc.date.accessioned | 2026-07-01T08:05:15Z | |
| dc.date.available | 2026-07-01T08:05:15Z | |
| dc.date.issued | 2013 | |
| dc.identifier.citation | Rodríguez Sáiz, Á., Manso Villalain, J. M., Gadea Sáinz, J., Gutiérrez González, S., Junco Petrement, C., y Calderón Carpintero, V. (2013). Obtaining building plaster used in building for forming ceiling, involves mixing recycled slag, additives and water in a blast furnace to obtain a homogeneous material [Patente]. | es |
| dc.identifier.uri | http://hdl.handle.net/20.500.12251/6636 | |
| dc.description.abstract | Obtaining building plaster used in building for forming ceiling, involves mixing recycled slag, additives and water in a blast furnace to obtain a homogeneous material. Water is added to the material and then the material is kneaded. 0-60% of gypsum slag and 0.35-0.40% added to the kneaded material. The materials are heated and processed at compression strength of 2.18 MPa, 3.94 MPa for 7 days and 0.81-7.16 MPa for 28 days. USE - Method for obtaining building plaster used in building for forming ceiling. ADVANTAGE - The method enables to obtain building plaster efficiently. | es |
| dc.language.iso | eng | es |
| dc.rights | Attribution-NonCommercial-NoDerivatives 4.0 Internacional | * |
| dc.rights.uri | http://creativecommons.org/licenses/by-nc-nd/4.0/ | * |
| dc.title | Obtaining building plaster used in building for forming ceiling, involves mixing recycled slag, additives and water in a blast furnace to obtain a homogeneous material | es |
| dc.type | patent | |
| dc.rights.accessRights | openAccess | es |
| dc.subject.keyword | Yeso | es |
| dc.subject.keyword | Reciclaje - Construcción | es |
| dc.subject.keyword | Escoria siderúrgica | es |
| dc.subject.unesco | 3312 Tecnología de Materiales | es |
| dc.subject.unesco | 3305 Tecnología de la Construcción | es |
| dc.subject.unesco | 3308.07 Eliminación de Residuos | es |
| dc.subject.unesco | 5312.03 Construcción | es |
| dc.subject.unesco | 3307.17 Dispositivos Termoeléctricos | es |
| dc.subject.unesco | 3305.33 Resistencia de Estructuras | es |
| dc.subject.unesco | 3313.04 Material de Construcción | es |
| dc.subject.unesco | 2211.19 Propiedades Mecánicas | es |